Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.014715 GPa @Temperature 1500 °C, Time 10800 sec |
2.1343 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories A50 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1350 °C, Time 10800 sec |
2.1343 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories BLC Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 110 °C, Time 86400 sec |
2.1343 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 - 0.016677 GPa @Temperature 1350 °C, Time 10800 sec |
2.1343 - 2.4188 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 110 °C, Time 86400 sec |
2.1343 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1500 °C, Time 10800 sec |
2.1343 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories LPCT-17PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1500 °C, Time 10800 sec |
2.1343 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories MMCT-85 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1350 °C, Time 10800 sec |
2.1343 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories MMCT-95 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1500 °C, Time 10800 sec |
2.1343 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories MMCT-95 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 250 °C |
2.1343 ksi @Temperature 482 °F |
|
Chosun Refractories SC40 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 1350 °C, Time 10800 sec |
2.1343 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories SFC-70R High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.014715 GPa @Temperature 110 °C, Time 86400 sec |
2.1343 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |