Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.010791 GPa @Temperature 1000 °C, Time 10800 sec |
1.5651 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories A80 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1000 °C, Time 10800 sec |
1.5651 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1000 °C, Time 10800 sec |
1.5651 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1500 °C, Time 10800 sec |
1.5651 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 110 °C, Time 86400 sec |
1.5651 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1500 °C, Time 10800 sec |
1.5651 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories LPCT-16DS Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 110 °C, Time 86400 sec |
1.5651 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories LPCT-17PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 110 °C, Time 86400 sec |
1.5651 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SFC-165 High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1000 °C, Time 10800 sec |
1.5651 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SW88 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.010791 GPa @Temperature 1500 °C, Time 10800 sec |
1.5651 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |