Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.008829 GPa @Temperature 110 °C, Time 86400 sec |
1.281 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories A40 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.008829 GPa @Temperature 500 °C, Time 10800 sec |
1.281 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories APC-50 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.008829 GPa @Temperature 1400 °C |
1.281 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-S81 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.008829 GPa @Temperature 1500 °C, Time 10800 sec |
1.281 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories CTC-60TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.008829 GPa @Temperature 110 °C, Time 86400 sec |
1.281 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SFC-60 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.008829 GPa @Temperature 1350 °C, Time 10800 sec |
1.281 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |