Mechanical Properties Metric English Comments
Puncture Energy 8.18 J
6.03 ft-lb
Dow Method
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)
AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre..