Polymer Property : Puncture Energy = 5.75 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 7.80 J
5.75 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 15 H2.0 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, good heat-ageing resistance