Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 25.0 - 35.0 J | 18.4 - 25.8 ft-lb | Average value: 28.0 J Grade Count:5 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Puncture Energy | 25.0 J | 18.4 ft-lb | ISO 6603-2 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
Puncture Energy | 25.0 J | 18.4 ft-lb | ISO 6603-2 |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Puncture Energy | 25.0 J | 18.4 ft-lb | ISO 6603-2 |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |
|||
Puncture Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |