Polymer Property : Puncture Energy = 55.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 38.0 - 55.0 J

@Temperature -40.0 - -40.0 °C
28.0 - 40.6 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 47.7 J Grade Count:12
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Puncture Energy 50.0 - 55.0 J
36.9 - 40.6 ft-lb
Average value: 51.5 J Grade Count:10
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..