Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 13.1 - 108 J | 9.66 - 79.7 ft-lb | Average value: 36.1 J Grade Count:6 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Puncture Energy | 13.1 J | 9.66 ft-lb | ISO 6603-2 |
Lanxess Durethan® DP 2801 000000 Nylon 66 PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free |