Puncture Energy 1.90 - 2.30 J
1.40 - 1.70 ft-lb
Average value: 2.22 J Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Puncture Energy 1.90 J

@Temperature -30.0 °C
1.40 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance
Puncture Energy 1.90 J

@Temperature -30.0 °C
1.40 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance
Puncture Energy 1.90 J

@Temperature -30.0 °C
1.40 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Puncture Energy 1.90 J

@Temperature -30.0 °C
1.40 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Puncture Energy 1.90 J
1.40 ft-lb
ISO 6603-2
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant