Mechanical Properties Metric English Comments
Flexural Modulus 0.0700 - 0.150 GPa
10.2 - 21.8 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 8299 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0700 GPa
10.2 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 8832 E BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0700 GPa
10.2 ksi
Plastcom SLOVAMID 66 HI/1 PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Flexural Modulus 0.0700 GPa
10.2 ksi
ISO 178
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: ..
Flexural Modulus 0.0700 GPa
10.2 ksi
ASTM D790
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Flexural Modulus 0.0700 - 36.2 GPa
10.2 - 5250 ksi
Average value: 2.51 GPa Grade Count:279
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Flexural Modulus 0.0700 GPa
10.2 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD915 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation materials. Flame retardant performance capable of meeting UL 1581 VW-1 require..
Flexural Modulus 0.0700 GPa
10.2 ksi
ASTM D790
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0700 GPa
10.2 ksi
ASTM D790
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Flexural Modulus 0.0700 - 0.276 GPa
10.2 - 40.0 ksi
Average value: 0.199 GPa Grade Count:13
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Copyright © lookpolymers.com All Rights Reserved