Mechanical Properties Metric English Comments
Flexural Modulus 4.80 - 5.50 GPa

@Temperature 90.0 - 90.0 °C
696 - 798 ksi

@Temperature 194 - 194 °F
Average value: 5.15 GPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Flexural Modulus 0.200 - 5.50 GPa
29.0 - 798 ksi
Average value: 2.20 GPa Grade Count:88
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Flexural Modulus 5.00 - 5.50 GPa
725 - 798 ksi
ASTM D790
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 0.305 - 5.50 GPa

@Temperature -40.0 - 120 °C
44.2 - 798 ksi

@Temperature -40.0 - 248 °F
Average value: 1.40 GPa Grade Count:8