Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Modulus | 3.30 - 3.30 GPa @Temperature 60.0 - 60.0 °C |
479 - 479 ksi @Temperature 140 - 140 °F |
Average value: 3.30 GPa Grade Count:2 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 3.20 - 3.30 GPa @Temperature 60.0 - 120 °C |
464 - 479 ksi @Temperature 140 - 248 °F |
Average value: 3.27 GPa Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Flexural Modulus | 2.96 - 3.30 GPa | 429 - 479 ksi | Average value: 3.16 GPa Grade Count:3 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |