Polymer Property : Flexural Modulus = 380 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00427 - 2.62 GPa
0.620 - 380 ksi
Average value: 0.743 GPa Grade Count:7
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m..
Flexural Modulus 0.586 - 2.62 GPa
85.0 - 380 ksi
Average value: 1.24 GPa Grade Count:214
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman 310 Utility Black PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman 330 White PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman 380 Grey PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..