Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.42 - 17.9 GPa | 206 - 2600 ksi | Average value: 2.49 GPa Grade Count:112 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Flexural Modulus | 3.51 - 17.9 GPa | 509 - 2600 ksi | Average value: 9.15 GPa Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 4.90 - 17.9 GPa | 710 - 2600 ksi | Average value: 10.6 GPa Grade Count:42 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Flexural Modulus | 1.10 - 17.9 GPa | 160 - 2600 ksi | Average value: 7.09 GPa Grade Count:96 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 2.76 - 17.9 GPa | 400 - 2600 ksi | Average value: 7.33 GPa Grade Count:131 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |