Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.647 - 1.37 GPa | 93.8 - 199 ksi | Average value: 1.06 GPa Grade Count:15 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 0.880 - 1.37 GPa | 128 - 199 ksi | ASTM D790 |
Zeus EFEP Tubing |