Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.689 GPa | 99.9 ksi | ASTM D790 |
Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding Impact Strength. TOTAL Polypropylene 7238 offers excellent impact strength, clarity and gloss.Lubricated 7238 offers superior core rod release for ease in processing.High Purity. 7238 features min.. |
|||
Flexural Modulus | 0.689 GPa | 99.9 ksi | ASTM D790 |
Diamond Polymers NPP11-0635 Medium Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 0.689 - 2.45 GPa | 99.9 - 355 ksi | Average value: 1.19 GPa Grade Count:65 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |