Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.686465 - 30.0 GPa @Temperature 150 - 260 °C |
99.5649 - 4350 ksi @Temperature 302 - 500 °F |
Average value: 6.87 GPa Grade Count:28 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |