Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.648 GPa | 94.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Flexural Modulus | 0.648 GPa | 94.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.648 GPa | 94.0 ksi | ASTM D790 |
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys |
|||
Flexural Modulus | 0.648 GPa @Thickness 19.0 mm |
94.0 ksi @Thickness 0.750 in |
ASTM D790 |
3A Composites Core Materials AIREX® PXc.420 Fiber-Reinforced Structural Foam AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu.. |