Mechanical Properties Metric English Comments
Flexural Modulus 0.634 - 1.90 GPa
92.0 - 276 ksi
Average value: 1.10 GPa Grade Count:3
Overview of materials for Nylon 6/69
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Flexural Modulus 0.634 GPa
92.0 ksi
ASTM D790
Multibase Multi-Flex® D 5308 X Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.634 GPa
92.0 ksi
Kuraray HYBRAR® PP3 Thermoplastic Rubber-Polypropylene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Flexural Modulus 0.634 GPa
92.0 ksi
ASTM D 790
Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69
Isocorâ„¢ 4011 is a high viscosity PA-6/69. This resin is specifically suited for applications requiring superior toughness and abrasion resistance. Isocorâ„¢ 4011 is also used in applicat..
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Flexural Modulus 0.634 GPa
92.0 ksi
ASTM D790
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane
Type: Estane® ALR E68D-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp..
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Flexural Modulus 0.634 GPa
92.0 ksi
1% secant; ASTM D790
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved