Mechanical Properties Metric English Comments
Flexural Modulus 6.26 GPa
908 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS
LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s).
Flexural Modulus 6.26 GPa
908 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66 (Asia Pacific)
LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release.