Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.13 GPa | 889 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66 LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 LNP* THERMOCOMP* PF005S is a compound based on Nylon 6 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF005S PA 6 (Asia Pacific) LNP* Thermocomp* PF005S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.13 GPa | 889 ksi | ISO 178 |
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 6.13 GPa @Temperature 65.0 °C |
889 ksi @Temperature 149 °F |
ASTM Test |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |