Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
NOVA Chemicals Sclair® 51-35BP HDPE Extrusion Resin Features: Medium molecular weight, excellent ESCR, excellent toughness, good processability, good chemical resistance.Applications: Extrusion on to metal pipes to produce a corrosion resistant coati.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos G36-24-149 MDPE with Carbon Black
(discontinued **) Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. .. |
|||
Flexural Modulus | 0.580 - 0.830 GPa | 84.1 - 120 ksi | Average value: 0.760 GPa Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M40 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-su.. |
|||
Flexural Modulus | 0.580 - 0.620 GPa | 84.1 - 89.9 ksi | ASTM D790 |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6322Z was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:High extrusion speedHigh thermal stabilityWide processing windowSuperior ele.. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D790 |
3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Flexural Modulus | 0.580 GPa | 84.1 ksi | ASTM D638 |
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |