Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437G40CL Glass Reinforced Coupled |
|||
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled |
|||
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G30CL Glass Reinforced Coupled |