Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.17 GPa | 750 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Nylex™ 4650 Polyamide + PP Mineral filler, 33% Filler by WeightForms: PelletsInformation provided by Multibase |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Flexural Modulus | 5.17 GPa @Thickness 3.17 mm |
750 ksi @Thickness 0.125 in |
ASTM D790 |
PTS 15GFR-BK PBT- Flame Retardant, 15% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PolyOne Edgetek® PK-10GF/000 Polyetheretherketone (PEEK) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.17 - 10.3 GPa | 750 - 1500 ksi | Average value: 8.71 GPa Grade Count:19 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | Tangent; ASTM D790 |
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 (Asia Pacific) LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS GF20 FR RD073 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Flame RetardantAppearance: RedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill® PP 0202 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill® PP 0225 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 5.17 GPa | 750 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0155 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |