Mechanical Properties Metric English Comments
Flexural Modulus 0.448 GPa
65.0 ksi
Tangent, 0.5 in/min; ASTM D790
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'..
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790(B)
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin
Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp..
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
Ecomass® 4702ZB92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
Ecomass® 4703ZB92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790
DuPont™ Surlyn® PC350 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for proces..
Copyright © lookpolymers.com All Rights Reserved