Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | ASTM D790 |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12 LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS (Asia Pacific) LNP* THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.45 GPa | 645 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |