Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.800 GPa | 551.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437M40CL Mica Reinforced Coupled |
|||
Flexural Modulus | 3.800 GPa | 551.1 ksi | ASTM D790 |
Aclo Accutech Polycarbonate POL050G10L Glass Reinforced |
|||
Flexural Modulus | 3.800 GPa | 551.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G20M10CL Glass/Mineral Reinforced Coupled |