Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced Information provided by Ravago. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1310G10 HB Polycarbonate, 10% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 2110 General Purpose Crystal Polystyrene
(discontinued **) Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 2590 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 3500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill and thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma .. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 3504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill an thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma r.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1504 High Heat Crystal Polystyrene Good balance of flow, strength and set up properties, Blue edge effect, USP Class VIApplications: Consumer electronics, Housewares, Cosmetic packagingExposure to gamma radiation in the 2.02-6.06 meg.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1600 High Heat Crystal Polystyrene High heat resistance, Moderate flow, Good balance of strength and set-upApplications: Foam extrusion, Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant e.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 3101 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Flexural Modulus | 3.448 GPa @Temperature 23.0 °C |
500.1 ksi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 2500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 3590 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable for difficult to fill and thin wall molding, Low residuals, USP Class VIApplications: Blending applications, Single service drinkware, Medical moldingExposure to g.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1200 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |
|||
Flexural Modulus | 3.448 GPa | 500.1 ksi | ASTM D790 |
Ineos Nova 1204 High Heat Crystal Polystyrene Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia.. |