Polymer Property : Flexural Modulus = 5.73 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0395 GPa
5.73 ksi
1% secant; ASTM D-790
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane  (discontinued **)
Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En..
Flexural Modulus 0.0395 - 0.0414 GPa
5.73 - 6.00 ksi
Average value: 0.0405 GPa Grade Count:3
Overview of materials for Silicone Polyurethane, Polycarbonate Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim..