Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Nylene® Norpex® AX20MRFR , 20% Mineral Reinforced, Flame Retardant Polyphenylene Ether Description: Norpex® AX20MRFR is a 20% mineral reinforced, flame retardant PPE. AX20MRFR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all opertin.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Flexural Modulus | 3.38 - 11.7 GPa | 490 - 1700 ksi | Average value: 5.50 GPa Grade Count:4 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Ineos Nova PS 3190 Crystal Polystyrene
(discontinued **) Information provided by Nova ChemicalsINEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 04003 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 HS NAT Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizerAppear.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | |
Asahi Kasei Thermylene® P-40TC-8100 Chemically Coupled Polypropylene Compound, 40% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
Asahi Kasei Thermofil P-40MI-0600 40% Mica Filled, Heat Stabilized Information provided by Asahi Thermofil |