Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
PolyOne Maxxam™ FR PE 161-1A Polyethylene, High Density (HDPE) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Microthene® F FN51900 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 818-073 offers the high environmental stress crack resistance characteristics of linear low density polyethylene with the processing properties needed for blowmolding and e.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% Secant; ASTM D790 |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 4107 C Black TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Microthene® G MN72200 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO X Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Techmer ES Plastiblend® POM CO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Techmer ES Luriblend® TPU T/AL27 Aramid Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber FilledAdditive: PTFE LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Arkema Group PLATAMID® 8020 Copolyamide Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group |
|||
Flexural Modulus | 0.276 - 0.414 GPa | 40.0 - 60.0 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |