Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.746 GPa | 398.3 ksi | ASTM D790 |
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66 Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon. |
|||
Flexural Modulus | 2.746 GPa @Temperature 260 °C |
398.3 ksi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is.. |
|||
Flexural Modulus | 2.746 GPa @Temperature 260 °C |
398.3 ksi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis-G40 ISO 40% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 car.. |