Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 25.77 GPa | 3738 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |