Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.224 GPa | 32.5 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0801 LDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |