Polymer Property : Flexural Modulus = 2982 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 20.56 GPa
2982 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched
LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
Flexural Modulus 20.56 GPa
2982 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched
LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding