Mechanical Properties Metric English Comments
Flexural Modulus 0.206 - 0.344 GPa
29.9 - 49.9 ksi
Secant 1%; ASTM D-790-95
Multibase Multi-Flex® TPO 4308 BLK
Data provided by Multibase.
Flexural Modulus 0.206 GPa
29.9 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 3104-8
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
SK Chemicals SKYPEL G155D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
SK Chemicals SKYPEL M555DH General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Flexural Modulus 0.206 GPa
29.9 ksi
ISO 178
Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent tear resistance. Molded and injected products for consumer use, such as airbag door covers, railwa..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Asia Technology Pioneers CAP 102 PP Nanocomposite
Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di..
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
SK Chemicals SKYPEL P155D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..