Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.196 - 2.55 GPa | 28.4 - 370 ksi | Average value: 2.06 GPa Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 0.196 GPa @Thickness 6.40 mm |
28.4 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 0.196 GPa @Thickness 6.40 mm |
28.4 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | ASTM D790 |
Kolon SPESIN® KP513 PBT Alloy Resin Excellent extrudable and SpinningApplications: Mono filamentInformation provided by API-Kolon. |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | ASTM D790 |
Kolon SPESIN® KP513UG PBT Alloy Resin Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon. |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | 200mm/min; ASTM D790 |
LG Chemical LUTENE LB4500 LDPE Extrusion Coating Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silico.. |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | 200mm/min; ASTM D790 |
LG Chemical LUTENE LB5000 LDPE Extrusion Coating Description: LUTENE LB5000 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB5000 is also noted for the excellent adhesion to porous a.. |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | 200mm/min; ASTM D790 |
LG Chemical LUTENE LB7500 LDPE Extrusion Coating Description: LUTENE LB7500 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB7500 is also noted for the excellent adhesion to porous a.. |
|||
Flexural Modulus | 0.196 GPa | 28.4 ksi | ASTM D790 |
SK Chemicals SKYPEL M555CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |