Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.89 GPa | 274 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl OP66UT105 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Flexural Modulus | 1.89 GPa @Thickness 6.40 mm |
274 ksi @Thickness 0.252 in |
ASTM D 790 |
SABIC Innovative Plastics Lexan® FL3000 PC Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp.. |
|||
Flexural Modulus | 1.89 GPa @Thickness 6.40 mm |
274 ksi @Thickness 0.252 in |
ASTM D 790 |
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific) Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Flexural Modulus | 1.89 - 2.96 GPa | 274 - 430 ksi | Average value: 2.47 GPa Grade Count:58 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ISO 178 |
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability.. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM Test |
BASF Ultramid® 8350 HS BK-102 PA6 (Dry) Ultramid 8350 HS BK-102 is a type 6, black pigmented, impact modified graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness
combined with a.. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.89 GPa | 274 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1245U CaCO3 Filled UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 1245U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |