Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.793 GPa | 260.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 5014 CU W Calcium Carbonate Filled Polypropylene Multi-Pro 5014 CU W is a calcium carbonate reinforced PP concentrate with balanced impact and stiffness properties. This product is specially formulated for lawn furniture, suitable for outdoor exp.. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Ineos Nova 5810 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | Secant @ 1% strain; ASTM D790 |
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro.. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |