Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.71 GPa | 248 ksi | ASTM D790 |
Nylene® PA6/6 Impact Modified 311 HS Nylon 6/6 Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | ASTM D790 |
Nylene® PA6/6 Impact Modified 4114 HS Nylon 6/6 High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | ASTM D790M |
DSM Somos® 7110 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Flexural Modulus | 1.71 GPa @Temperature 23.0 °C |
248 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H02C-00 Polypropylene Homopolymer This is a low flow rate, high clarity homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging. Applications that require good see-through clarity combined with good hea.. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | ISO 178 |
Solvay TECHNYL® A 50H1 PA66, Conditioned Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10 LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® 627L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Flexural Modulus | 1.71 GPa | 248 ksi | ASTM D790 |
Diamond Polymers NYLON 6615 HS Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |