Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.55 GPa | 2400 ksi | ASTM D790 |
PlastiComp Complet® LCF30-PA66 30% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Modulus | 16.55 GPa | 2400 ksi | ASTM D-790 |
PlastiComp Velocity® LGF50-PA66 High Flow Nylon 66, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | Crosswise; ASTM D790 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Chase Plastics CP Pryme® NNN260L (Dry) Nylon 66/6 Copolymer, 60% Glass Fiber Reinforced Features: Good chemical resistanceGood compressive strengthGood creep resistanceGood dimensional stabilityGood flowGrease resistantOil resistantHigh rigiditySolvent resistantHigh tensile strengthHig.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method.. |