Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.162 GPa | 23.5 ksi | ASTM D790 |
Toyobo PELPRENE™ P90B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Flexural Modulus | 0.162 GPa | 23.5 ksi | ASTM D790 |
Toyobo PELPRENE™ P90BD Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |