Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.159 GPa | 23.1 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips 1008.5 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 14200Characteristics: Excellent Flexibility, Excellent Flow, Good Warping Resistance, Moderate Mold Release, Moderate ESCRApplications:.. |
|||
Flexural Modulus | 0.159 GPa | 23.1 ksi | ASTM D790 |
DuPont™ Surlyn® 8670 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8670 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Flexural Modulus | 0.159 GPa | 23.1 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |