Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.448 GPa | 210.0 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-6507 Multi-Flex® D 6507 is a mineral filled TPO polypropylene compound designed for applications requiring high impact and moderate stiffness.Data provided by Multibase. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | tangent; ASTM D790 |
Entec Hypro™ PPC-T10 Copolymer Polypropylene, 10% Talc Reinforced Information provided by Entec |
|||
Flexural Modulus | 1.448 GPa | 210.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |