Polymer Property : Flexural Modulus = 2099 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66
LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific)
LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Flexural Modulus 14.47 GPa
2099 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific)
LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non..
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66
LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare.
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific)
LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber.
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Asia Pacific)
LNP* Stat-kon* DEL36 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, , Internally Lubricated.