Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.1 GPa | 1750 ksi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 RM LE 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables, Low Moisture Absorption and LubricatedInf.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 12.1 GPa | 1750 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66 LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare. |
|||
Flexural Modulus | 12.07 GPa | 1750 ksi | ASTM D790 |
E-Polymers SEPAZ® V235A 35% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |