Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.14 GPa | 165 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM120LN Polypropylene Impact Copolymer COPYLENE™ CM120LN is a high impact copolymer formulated with antistat and nucleated for demanding injection molding applications.Applications: Injection molding applications including crates, totes.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 990 TPO
(discontinued **) Description: DEXFLEX® 990 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, and excellent pr.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech SP-1510 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3312E Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312E is a clarified, medium flow random copolymer with fast cycle time and easy mold release. It is designed for injection .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6520A Injection Molding Polypropylene Impact CopolymerApplications: Closures, Housewares, Small Appliance ApplicationsFormolene 6520A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property b.. |
|||
Flexural Modulus | 1.14 - 6.21 GPa | 165 - 900 ksi | Average value: 3.16 GPa Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |