Polymer Property : Flexural Modulus = 162.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.118 GPa
162.2 ksi
2% Secant; 12.5 mm/min; ASTM D790
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c..