Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.5 GPa | 1530 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF15 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.55 GPa | 1530 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 10.55 GPa | 1530 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber. |
|||
Flexural Modulus | 10.55 GPa | 1530 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Flexural Modulus | 10.55 GPa | 1530 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 10.55 GPa | 1530 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific) LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber. |