Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 GPa | 153 ksi | Tangent; ASTM D790 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.05 - 12.4 GPa | 153 - 1800 ksi | Average value: 9.87 GPa Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | 2% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos L40N-00 Polypropylene Impact Copolymer L40N-00 is a nucleated high flow polypropylene, medium impact copolymer for injection molding applications. This resin exhibits an excellent balance of resin flow and mechanical properties. This res.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos R35C-02 Polypropylene Random Copolymer Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |